Tshuab ziab khaub ncaws
Cov ntaub ntawv yasmuaj hygroscopic pawg xws li amide, ester, ether, thiab cyanide hauv lawv cov qauv molecular, muab lawv nyiam nqus dej noo. Qhov kev nqus dej no ua rau muaj qhov sib txawv ntawm cov dej ntsiab lus. Thaum cov dej noo ntau dhau ib theem, cov teeb meem xws li nyiaj streaks, shrinkage pores, thiab npuas yuav tshwm nyob rau hauv cov khoom, thiab cov khoom yuav degrade.
Cov yas uas yooj yim nqus dej muaj xws li PA, PC, PMMA, PET, PSF (PSU), PPO, thiab ABS. Raws li txoj cai, cov ntaub ntawv no yuav tsum tau qhuav ua ntej molding. Cov txheej txheem ziab qhuav txawv nyob ntawm cov yas; Table 2-1 qhia txog kev ziab kom qhuav rau cov khoom siv yas.

Muaj ntau txoj hauv kev kom qhuav cov yas, xws li circulating cua kub kom qhuav, infrared cua sov kom qhuav, nqus cua sov kom qhuav, thiab airflow kom qhuav.
Nws yuav tsum tau muab sau tseg tias cov khoom qhuav yuav tsum tau tiv thaiv los ntawm re- absorbing noo noo. Table 2-2 qhia txog qhov tso cai noo noo cov ntsiab lus ntawm cov yas ua ntej molding.

Preheating ntawm inserts
Vim tias cov yas thiab cov hlau muaj qhov sib txawv ntawm cov thermal conductivity ntau heev- cov yas muaj cov thermal conductivity qis dua, cov coefficient ntawm linear expansion ntau dua, thiab cov molding shrinkage npaum li cas, thaum cov hlau muaj qhov me me shrinkage npaum li cas -cov khoom yas nrog cov hlau ntxig yog qhov ua rau tawg nyob ib ncig ntawm cov khoom siv, uas ua rau cov khoom lag luam qis dua.
Txhawm rau daws qhov teeb meem no, lub thickness ntawm cov yas nyob ib ncig ntawm qhov ntxig yuav tsum tau nce ntxiv thaum lub sij hawm tsim cov khoom yas. Preheating cov hlau ntxig thaum ua tiav yuav txo qhov kub ntawm qhov sib txawv ntawm cov yas molten thiab cov hlau ntxig, ua rau kom txias ntawm cov yas nyob ib ncig ntawm qhov ntxig thiab ua kom muaj qhov sib txawv ntau dua, yog li tiv thaiv kev ntxhov siab ntau dhau ntawm qhov ntxig.

Lub preheating ntawm inserts nyob ntawm seb cov khoom ntawm cov yas, qhov loj thiab hom ntawm inserts. Rau cov yas uas muaj cov saw hlau tsis zoo, xws li PC, PS, PSF, thiab PPO, preheating yog tsim nyog thaum muaj cov khoom siv. Txawm li cas los xij, rau cov yas uas hloov tau cov saw hlau molecular thiab cov ntxig me me, tsis tas yuav tsum tau preheating.
Qhov dav dav preheating kub rau inserts yog 110-130 degree, tab sis rau cov ntaub ntawv xws li txhuas thiab tooj liab, nws tuaj yeem nce mus rau 150 degree.
Kev xaiv tus neeg tso tawm
Rau qee yam khoom siv yas nrog cov qauv tso tawm nyuaj, tus neeg sawv cev tso tawm yuav tsum tau muab txau rau hauv cov tub ntxhais pwm thaum lub sij hawm txhaj tshuaj molding los pab txhawb qhov ejection ntawm cov khoom yas los ntawm cov tub ntxhais pwm.
Cov tshuaj tso tawm ib txwm muaj xws li zinc stearate, roj dawb, thiab roj silicone. Zinc stearate tuaj yeem siv rau ntawm cov yas feem ntau tsuas yog polyamides. Cov roj dawb muaj txiaj ntsig zoo dua li tus neeg sawv cev tso rau polyamides. Silicone roj siv tau zoo tab sis tsis yooj yim rau siv.