Txhaj tshuaj molding txheej txheem rau pob tshab yas

Dec 19, 2025

Tso lus

◆Cov yam ntxwv ntawm cov pob tshab yas

Transparent plastics thiab lawv cov kev txhaj tshuaj molding

transparent plastics

 

Nrog kev nce qib hauv cov ntaub ntawv tshawb fawb thiab kev txhim kho, kev nce ntxiv ntawm cov khoom siv kho qhov muag tsim nyog rau kev tsim cov khoom pob tshab. Kev siv cov lo ntsiab muag kho qhov muag, dav siv hauv cov khoom siv kho qhov muag nrog cov kev xav tau zoo thiab cov tshuab txhaj tshuaj molding complex, ua piv txwv, raws li qhia hauv daim duab, cov khoom siv tshuaj molding rau cov lo ntsiab muag zoo tib yam feem ntau xaiv rau nws tus nqi qis, kev ua haujlwm siab, muaj zog ruaj khov, thiab kev xa tawm siab. Piv nrog rau cov ntaub ntawv raw khoom rau cov yas lo ntsiab muag zoo tib yam, cov kev cai rau kev txhaj tshuaj molding cov ntaub ntawv rau cov duab optics yas lo ntsiab muag yog qhov nruj dua. Tsis tsuas yog yuav tsum tau cov khoom siv yas raw khoom muaj cov yam ntxwv xws li siab pob tshab, zoo txhua yam khoom, muaj zog stability, thiab zoo flowability, tab sis cov khoom xaiv yuav tsum tau raws li cov kev ua tau zoo yam ntxwv xws li refractive index.

 

Feem ntau siv cov ntaub ntawv txhaj tshuaj molding rau cov duab kho qhov muag iav lo ntsiab muag suav nrog polymethyl methacrylate (PMMA), polycarbonate (PC), thiab cyclic olefin polymers (COP). Ntawm cov no, siab -pob tshab PMMA yog dav siv nyob rau hauv kev txhaj tshuaj molding ntawm yas lo ntsiab muag. PMMA tsis yog siv rau hauv kev tsim cov khoom nruab nrab - mus rau -low precision loj- txoj kab uas hla yas lo ntsiab muag, xws li condenser lo ntsiab muag, Fresnel lo ntsiab muag, projection lo ntsiab muag, thiab automotive headlight lo ntsiab muag, tab sis kuj nyob rau hauv siab -precision yas lo ntsiab muag, xws li laser tshuab luam ntawv lo ntsiab muag, lub koob yees duab lo ntsiab muag, lub xov tooj ntawm tes lo ntsiab muag, thiab CD / DVD nyeem lo ntsiab muag. PMMA muaj lub zog siab thiab hardness, nrog rau cov khoom siv kho qhov muag xws li tus lej Abbe siab thiab qis birefringence. Txawm li cas los xij, PMMA tseem nthuav tawm ntau qhov kev sib tw ua cov khoom siv yas rau cov lo ntsiab muag kho qhov muag. Piv txwv li, nyob rau hauv cov huab cua ntub dej, PMMA qhov nqus dej ua rau muaj kev hloov pauv hauv qhov ntsuas qhov ntsuas ntawm lub lens yas, uas ua rau lub ntim nthuav dav thiab hloov pauv mus rau tag nrho cov qauv qhov ntev. Tsis tas li ntawd, PMMA lub iav hloov pauv kub yog 100 degree, thiab qhov kub tsis kam ntawm cov iav lo ntsiab muag yog qhov tsis zoo, uas cuam tshuam qhov kev thov ntau ntawm PMMA.

 

Polycarbonate (PC) yog cov khoom siv kho qhov muag uas nquag siv, dav siv nyob rau hauv tsheb lub teeb tsom teeb, kab teeb -diffusing lo ntsiab muag, thiab lwm yam lo ntsiab muag kho qhov muag. PC muaj lub siab transparency, kub tsis kam, siab zog, thiab siab refractive Performance index, thiab suav hais tias yog ib qho ntawm cov ntaub ntawv yas nrog lub zog zoo tshaj plaws. Txawm li cas los xij, PC lo ntsiab muag tseem muaj qhov tsis zoo. Piv txwv li, photoelastic coefficient ntawm PC lo ntsiab muag yog ob peb zaug siab dua li PMMA, uas ua rau muaj kev cuam tshuam birefringence uas ua rau muaj kev cuam tshuam loj rau cov duab kho qhov muag ntawm lub lens yas. Tsis tas li ntawd, cov khoom siv PC muaj qhov loj me me, ua rau cov iav lo ntsiab muag muaj qhov cuam tshuam rau deformation, nrog rau qib deformation ntau dua li PMMA.

transparent plastics

 

transparent plastics

 

Cyclic olefin polymers (COPs) yog lub nplhaib- ntiv tes polymers ua ke siv cyclic olefins ua monomers. COPs muaj cov pob tshab siab, tsis tshua muaj hygroscopicity, tsis tshua muaj birefringence, thiab kev ua haujlwm zoo. Tsis tas li ntawd, COPs pom zoo ib puag ncig kev ruaj ntseg, tseem tsis tau hloov pauv txawm tias nqus dej noo, thiab nquag siv los hloov PMMA hauv cov yas. Txawm li cas los xij, COPs yog kim heev, raug nqi kwv yees li kaum npaug tshaj PMMA. Siv COPs ua cov khoom siv tshuaj molding ua rau cov nqi tsim khoom ntawm cov lo ntsiab muag yas.

 

Feem ntau, lo ntsiab muag ua los ntawm PC muaj qhov tseem ceeb birefringence, ua rau nws nyuaj los lav cov duab zoo. COP thiab PMMA muab qhov zoo sib xws ntawm cov khoom siv kho tshuab thiab cov qauv kev ruaj ntseg. Txawm li cas los xij, COP yog kim heev, nce nqi tsim khoom thiab ua txhaum txoj cai ntawm kev lag luam. PMMA, ntawm qhov tod tes, yog tus pheej yig thiab muaj kev lag luam loj, ua rau nws tsim nyog rau kev tsim khoom qis - nqi, siab - kev ua tau zoo imaging optical yas lo ntsiab muag. Tsis tas li ntawd, PMMA cov dej ntws ntws tuaj yeem txhim kho los ntawm kev hloov pauv cov txheej txheem kev txhaj tshuaj molding, tso cai rau kev rov ua dua ntawm kev txhaj tshuaj pwm qhov chaw morphology.

 

 

Txhaj tshuaj molding tshuab rau pob tshab yas

 

 

Vimpob tshab yasxav tau lub teeb pom kev zoo siab, qhov zoo ntawm cov khoom yas yuav tsum tau tswj nruj me ntsis. Cov teeb meem xws li blemishes, pores, whitening, haze, black spots, discoloration, thiab tsis zoo gloss yog tsis tsim nyog. Yog li ntawd, tag nrho cov txheej txheem txhaj tshuaj molding yuav tsum tau ua tib zoo saib xyuas thiab nruj, txawm tias tshwj xeeb, yuav tsum muaj cov khoom siv raw, khoom siv, pwm, thiab txawm tias tsim khoom.

transparent plastics

Thib ob, vim qhov siab melting point thiab tsis zoo flowability ntawm pob tshab yas, kev kho kom zoo rau cov txheej txheem tsis xws li tshuab kub, txhaj tshuaj, thiab txhaj tshuaj ceev yog feem ntau tsim nyog los xyuas kom meej qhov zoo. Qhov no ua kom cov pwm puv tag nrho yam tsis muaj kev ntxhov siab sab hauv uas tuaj yeem ua rau cov khoom deformation thiab tawg. Cov ntu hauv qab no txheeb xyuas cov ntsiab lus tseem ceeb hais txog kev npaj cov khoom siv raw, cov khoom siv thiab cov pwm yuav tsum tau ua, cov txheej txheem txhaj tshuaj molding, thiab kev tuav raw khoom.

 

Cov ntsiab lus tseem ceeb ua ntej txhaj tshuaj molding

 

Raw Material Npaj thiab ziab

Txij li txawm tias me ntsis impurity hauv cov yas tuaj yeem cuam tshuam rau cov khoom pob tshab, nws yog ib qho tseem ceeb uas yuav tsum muaj lub kaw ntom nti thaum lub sij hawm khaws cia, kev thauj mus los, thiab pub mis kom paub meej tias cov ntaub ntawv raw yog huv si. Hauv particular, muaj cov dej noo nyob rau hauv cov ntaub ntawv raw tuaj yeem ua rau tsis zoo thaum cua sov, yog li kev ziab kom qhuav yog qhov tseem ceeb. Thaum txhaj tshuaj molding, lub tshuab ziab khaub ncaws yuav tsum tau siv rau kev pub mis. Nws tseem yog ib qho tseem ceeb uas yuav tsum nco ntsoov tias cov huab cua qhia thaum lub sij hawm ziab yuav tsum tau lim thiab dehumidified kom tsis txhob muaj kab mob ntawm cov khoom siv raw.

 

Ntxuav lub thoob, ntsia hlau thiab accessories

transparent plastics

 

Txhawm rau tiv thaiv cov khoom siv raw khoom sib kis thiab sib sau ua ke ntawm cov khoom qub lossis impurities hauv cov ntsia hlau thiab nws cov khoom siv, tshwj xeeb yuav tsum tau them nyiaj tshwj xeeb los tiv thaiv cov khoom qub uas tsis zoo thermal stability. Ua ntej thiab tom qab siv, lub tshuab txhaj tshuaj molding yuav tsum tau muab ntxuav kom huv si nrog lub tshuab nqus tsev ntxhua khaub ncaws kom ntseeg tau tias txhua qhov kev txhaj tshuaj tsis muaj impurities. Yog tias tsis muaj lub tshuab ntxhua khaub ncaws, PE lossis PS yas tuaj yeem siv los ntxuav cov ntsia hlau. Thaum lub sijhawm kaw ib ntus, txhawm rau tiv thaiv kev degradation los ntawm kev cuam tshuam ntev ntawm cov khoom siv raw mus rau qhov kub siab, lub tshuab ziab khaub ncaws thiab lub thoob kub yuav tsum tau qis dua. Yog tias tsim cov PC, PMMA, lossis lwm yam yas, lub thoob kub yuav tsum raug txo kom qis dua 160 degree. Tsis tas li ntawd, thaum siv PC raws li cov khoom siv raw, lub hopper ziab kub yuav tsum raug txo kom qis dua 100 degree.

 

Cov teeb meem xav txog hauv kev tsim pwm (nrog rau cov khoom tsim)

Txhawm rau tiv thaiv cov yas molding tsis zoo, qhov tsis zoo ntawm qhov chaw, thiab kev puas tsuaj los ntawm qhov tsis zoo rov qab los yog qhov tsis sib xws, cov ntsiab lus hauv qab no feem ntau yuav tsum tau txiav txim siab thaum tsim pwm.

01

Lub thickness ntawm phab ntsa yuav tsum zoo ib yam li qhov ua tau, thiab lub kaum sab xis yuav tsum loj txaus.

02

Cov ntu kev hloov pauv yuav tsum maj mam thiab ua kom zoo sib npaug kom tsis txhob muaj cov kaum ntse ntse thiab cov npoo, tshwj xeeb tshaj yog rau cov khoom siv PC, uas yuav tsum tsis muaj qhov tsis zoo.

03

Lub rooj vag thiab khiav yuav tsum dav thiab luv li sai tau, thiab lub rooj vag txoj hauj lwm yuav tsum tau teem raws li lub shrinkage thiab solidification txheej txheem. Lub qhov dej txias txias yuav tsum tau ntxiv yog tias tsim nyog.

04

Cov pwm saum npoo yuav tsum du nrog cov roughness tsawg (zoo dua hauv qab 0.8µm).

05

Yuav tsum muaj cov vents txaus thiab cov channel kom sai sai tshem tawm cov huab cua thiab cov pa tawm ntawm cov khoom molten.

06

Tsuas yog PET, phab ntsa tuab yuav tsum tsis txhob nyias dhau, feem ntau tsis pub tsawg tshaj 1 hli.

 

Cov teeb meem yuav tsum tau xav txog hauv Kev Txhaj Tshuaj Molding Txheej Txheem (xws li Kev Txhaj Tshuaj Molding Tshuab Yuav Tsum Tau)

Txhawm rau txo qhov kev ntxhov siab sab hauv thiab qhov tsis zoo ntawm qhov chaw, cov hauv qab no yuav tsum tau xav txog hauv cov txheej txheem txhaj tshuaj molding:

Siv lub tshuab txhaj tshuaj molding nrog rau cov ntsia hlau tshwj xeeb thiab qhov ntsuas kub sib cais - tswj lub nozzle.

01

Kev Txhaj Tshuaj Kub Kub: Qhov kev txhaj tshuaj ntau dua yog qhov zoo dua, yog tias cov yas resin tsis decompose.

02

Kev Txhaum Cai: Feem ntau siab dua kom kov yeej cov viscosity siab ntawm cov yaj, tab sis cov siab ntau dhau tuaj yeem ua rau muaj kev ntxhov siab sab hauv, ua rau kev nyuaj siab thiab deformation.

03

Kev txhaj tshuaj nrawm: Feem ntau qis dua, thaum ua kom cov pwm puv, qhov zoo yog siv ntau-theem txhaj tshuaj ntawm qeeb- nrawm- qeeb.

04

Tuav lub sij hawm thiab Moulding voj voog: luv dua, thaum ua kom cov khoom ntim thiab tiv thaiv cov cim dab dej thiab npuas, kom txo tau lub sij hawm nyob ntawm cov khoom molten hauv lub thoob.

05

Screw Speed ​​​​thiab Back Pressure: Tsawg li sai tau, thaum ua kom cov yas zoo, kom txo tau qhov delamination.

06

Pwm kub: Qhov zoo ntawm cov khoom cua txias muaj kev cuam tshuam zoo, yog li pwm kub yuav tsum raug tswj kom raug. Yog tias ua tau, pwm kub yuav tsum siab dua.

07

 

Lwm yam teeb meem

 

Txhawm rau tiv thaiv qhov tsis zoo ntawm qhov tsis zoo, cov pwm tso tawm cov neeg ua haujlwm yuav tsum tau siv me ntsis thaum txhaj tshuaj molding; tus nqi ntawm cov khoom siv rov ua dua yuav tsum tsis pub tshaj 20%. Tsuas yog PET, tag nrho cov khoom yuav tsum tau ua tom qab- kho kom txo tau qhov kev ntxhov siab sab hauv. PMMA yuav tsum tau qhuav hauv huab cua kub ntawm 70-80℃rau 4 teev; PC yuav tsum tau ua kom sov hauv huab cua huv, glycerin, kua paraffin, thiab lwm yam, ntawm 110-135℃rau ib lub sijhawm nyob ntawm cov khoom, qee zaum xav tau ntau tshaj 10 teev. PET yuav tsum dhau los ua cov txheej txheem biaxial stretching kom ua tiav cov khoom zoo.

transparent plastics