SABIC Launch Ib Tug Tshiab Resin Los Txo Kev Ua qias tuaj thiab txhawb kev lag luam ncig

May 18, 2022

Tso lus

Lub Tsib Hlis 16, SABIC, lub tuam txhab muaj ntau hom tshuaj lom neeg thoob ntiaj teb, tau tshaj tawm LNP ™ ELCRIN ™ Wf0061biq resin, cov khoom siv tshiab, siv cov khib nyiab hauv dej hiav txwv PET (polyethylene terephthalate) yas fwj ua raw cov ntaub ntawv thiab tau upgraded thiab reconstituted rau hauv PBT (polybutylene terephthalate) resin. los ntawm kev siv tshuaj. Marine plastics hais txog cov khoom pov tseg yas uas tsis tswj tau zoo nyob rau hauv 30 mais (50 mais) los ntawm ntug dej hiav txwv, thiab lawv muaj feem yuav nkag mus rau hauv dej hiav txwv.


Raws li tus tswv cuab tshiab ntawm SABIC LNP elcrin IQ tshuaj kho dua tshiab cov khoom siv txuas ntxiv mus rau tsev neeg, cov khoom lag luam no pab txhawb kev lag luam ncig thiab tuaj yeem siv los ua ib qho kev hloov pauv rau thawj PBT resin. LNP elcrin wf0061biq resin tseem yuav tsum tau siv rau hauv cov khoom siv hluav taws xob siv hluav taws xob, xws li kiv cua vaj tse, cov khoom siv hluav taws xob thiab cov vaj tsev ntawm cov khoos phis tawj thiab lub rooj zaum hauv tsheb.



Sanjay Mishra, tus thawj tswj hwm ntawm R & D thiab thev naus laus zis ntawm SABIC cov ntaub ntawv tshwj xeeb, hais tias: "Peb tab tom ua kom cov khoom lag luam zoo ntawm LNP elcrin IQ. Tib lub sijhawm, peb tseem nquag rov ua dua cov tsiaj pov tseg uas siv los tsim cov ntaub ntawv no. Peb cia siab tias yuav 'Txuag' ntau cov yas los ntawm dej hiav txwv thiab pab peb cov neeg siv khoom ntxiv cov khoom siv rov ua dua tshiab rau lawv cov khoom kom ua tiav lawv lub hom phiaj carbon neutralization, thaum ua tau raws li qhov xav tau ntawm cov neeg siv khoom xav tau ntau ntxiv rau kev ruaj ntseg hauv 10 xyoo tom ntej, peb cia siab tias 10 billion. lub raj mis yas yuav tsum tau kho dua tshiab thiab ua rau muaj teeb meem kev ua tau zoo Cov khoom siv ruaj khov tsim muaj txiaj ntsig ntau rau cov neeg siv khoom.


SABIC tau cog lus los ua haujlwm nrog tag nrho cov khoom siv yas los nrhiav cov kev daws teeb meem tshiab rau cov teeb meem ib puag ncig sai zuj zus, suav nrog kev txo qis cov khoom pov tseg hauv hiav txwv thiab pab kom ua tiav cov pa roj carbon emissions. "


Kev ua tau zoo heev, pab kev lag luam ncig


Lub brand-new LNP elcrin wf0061biq yog iav fiber reinforced PBT khoom nrog bromine thiab chlorine dawb nplaim retardant yam ntxwv, uas ua tau raws li UL94 V0 (0.8mm thickness) thiab F1 nplaim retardant qauv. Nws kuj muaj qhov ua tau zoo thaum tshav kub kub, toughness thiab nruj, thiab nws cov fluidity siab kuj ua rau nws zoo tagnrho cov khoom siv rau sab nraum zoov nyias-phab ntsa tsim daim ntaub ntawv xws li cov khoom siv hluav taws xob.


Txhua LNP elcrin IQ cov ntaub ntawv tuaj yeem siv los ua cov khoom hloov pauv rau PBT ib txwm siv los pab cov tuam txhab txhim kho kev ruaj ntseg ntawm cov khoom kawg. SABIC's proprietary chemical upgrading thev naus laus zis tuaj yeem rov ua cov khoom pov tseg marine rau hauv PBT cov ntaub ntawv piv rau cov khoom qub. Cov txheej txheem no dhau mus dhau cov txheej txheem kho tshuab rov qab ib txwm nyob rau hauv cov nqe lus ntawm cov khoom zoo thiab kev ua tau zoo sib xws.


Darpan Parikh, tus thawj coj ntawm Asmeskas kev lag luam ntawm SABIC cov ntaub ntawv tshwj xeeb, tau hais tias: "Ib qho kev ntsuas kev ua neej nyob sab hauv raws li ISO 14040 / 14044 qhia tias LNP elcrin wf0061biq hloov cov khoom tuaj yeem txo nws cov pa roj carbon monoxide los ntawm 14 feem pua ​​thiab nws xav tau lub zog xav tau. Kev txo qis los ntawm 25 feem pua ​​​​piv rau cov iav fiber reinforced thawj PBT. Siv peb cov resin los hloov cov khoom tseem ceeb, cov neeg siv khoom tuaj yeem txo qhov cuam tshuam rau ib puag ncig los ntawm kev rov siv cov yas pov tseg thiab tshem tawm cov khoom siv halogen. "