Yas Diffuser Rau Led specification
Khoom siv: Polycarbonate 2805
Xim: Ntshiab
Qhov siab: 10mm
Dav: 70mm
Thickness: 1.5 hli
Qhov hnyav: 140g / m
Bayer 2805 qhia
Keeb kwm: Bayer, Germany
Nta: nruab nrab viscosity txhaj tshuaj qib, yooj yim demoulding Muab cov cua sov ua haujlwm zoo, zoo pob tshab, muaj zog cuam tshuam thiab lwm yam khoom siv lub cev thiab cov khoom siv kho tshuab. PC muaj kev ua tau zoo tshaj plaws, tshwj xeeb tshaj yog muaj kev cuam tshuam zoo, pob tshab thiab qhov ruaj khov;
PC muaj cov cuab yeej zoo heev. Dab tsi yog qhov zoo tshaj plaws yog nws qhov cuam tshuam lub zog thiab qhov ntev stability. Nws tseem tuaj yeem tuav lub zog txhua yam hauv qhov kub thiab txias. Nws qhov tsis zoo yog qaug zog qaug zog thiab hnav tsis kam, thiab nws yooj yim los tsim kev ntxhov siab tawg. Nws muaj qhov ua kom sov zoo. Nws qhov kub decomposition yog siab dua 300 degree, thiab nws lub sijhawm ua haujlwm kub tuaj yeem siab txog 120 degree. Nyob rau tib lub sijhawm, nws muaj qhov ua tau zoo txias. Lub embrittlement kub yog tsawg li - 100 degree , thiab nws cov kev pab mus sij hawm ntev kub yog - 60 degree - 120 degree . Hluav taws xob rwb thaiv tsev kev ua tau zoo, nyob ze los yog sib npaug rau cov tsiaj zoo heev, zoo aging kuj thiab kub aging kuj. PC yog yooj yim nqus dej, thiab cov dej nyob rau hauv high-kub txheej txheem ntawm kev tsim thiab kev ua yuav kuj hydrolyze thiab degrade PC, uas yuav cuam tshuam rau lub cev, lub cev thiab txhua yam khoom ntawm cov khoom. Yog li ntawd, kev tswj cov dej ntsiab lus yog ib qho ntawm cov yuam sij kom ntseeg tau cov khoom zoo;
Cov txheej txheem ua:
Ci cov khoom ntawm 120 ° C rau li 4 teev;
Qhov kub ntawm lub tes tsho txhaj tshuaj yog nyob nruab nrab ntawm 230 ~ 320 ° C;
Cov pwm kub yog 70 ~ 120 ° C;
Tsis txhob cia cov kua nplaum kub yaj nyob rau hauv lub raj cua sov kom ntev thaum lub sij hawm txhaj tshuaj;
Daim ntawv thov: kev ua tau zoo ntawm PC yuav zoo heev thiab tau siv dav. Nws yog tsuas yog siv nyob rau hauv lub tshav pob ntawm siab transparency thiab muaj feem xyuam rau lub zog. Niaj hnub no, cov khoom siv optical disc yog ib qho tseem ceeb ntawm kev siv PC. Lub lag luam muaj peev xwm nthuav dav siv PC hauv kev lag luam tsheb tsim kuj tseem loj. Nws tuaj yeem siv los tsim cov teeb taws hauv tsheb, teeb sab hauv, teeb lub teeb, tsom iav, tsom iav, tsheb iav, sab hauv thiab sab nrauv kho kom zoo nkauj thiab ntsuas vaj huam sib luag;
Hauv kev lag luam hluav taws xob thiab hluav taws xob, nws tuaj yeem siv rau kev xaim hluav taws xob ntawm cov khoom siv hluav taws xob tsawg, ntau yam insulating plug-ins, lub tes tsho insulating, tshuab twj tiv thaiv lub cev muaj zog hloov, hollow cib plhaub, ntsuas plhaub thiab cov khoom siv hauv chaw ua haujlwm, thiab tseem tuaj yeem ua tau. tsim cov khoom tseem ceeb ntawm polymer optical fiber;
PC tuaj yeem hloov iav thiab hlau thiab siv rau hauv cov khoom siv hauv tsev thiab lwm yam haujlwm
Yas Diffuser Rau Led duab: