Cia kuv pib nrog ib yam dab tsi uas daig nrog kuv.
Xyoo tas los kuv tau mus xyuas ibkev tsim khoom profilecog hauv Dongguan. Tus thawj saib xyuas kev cob qhia, Qub Zhou, taw tes rau ntawm lub tshuab extruder thiab hais rau kuv tias: "Koj pom qhov no? Txoj ntsiab cai yog qhov yooj yim tuag. Tsis txawv ntawm kev nyem cov tshuaj txhuam hniav tawm ntawm lub raj."
Kuv xav tias nws dag.

Hloov tawm, tom qab tau nkag mus rau hauv kev lag luam no, nws tsis yog lawm -tsawg kawg tsis yog hais txog lub ntsiab lus tseem ceeb. Extrusion molding, raws li lub npe qhia, yuav tsum nias ib yam khoom los ntawm qhov qhib los ua ib qho duab. Ib yam li thaum koj nyem qhov kawg ntawm cov tshuaj txhuam hniav, cov tshuaj txhuam hniav extruded zoo li lub qhov me me. Lub hauv paus ntsiab lus ntawm cov yas extrusion molding zoo ib yam, tshwj tsis yog tias koj tus ntiv tes hloov los ntawm cov ntsia hlau rotating, cov tshuaj txhuam hniav ua cov yas molten, thiab lub raj qhib los ua qhov tseeb -machined pwm.
Tab sis "yooj yim" txhais tau tias qee yam txawv heev thaum koj tham txog kev tsim khoom lag luam.
Yog li dab tsi yog peb extruding ntawm no
Profile extrusion yog txheej txheem ntawm kev tsim cov yas txuas ntxiv los ntawm extrusion. Nws tsis suav nrog cov ntawv lossis cov khoom ua yeeb yaj kiab. Ntau tus neeg tsis meej pem "extrusion" raws li lub tswv yim dav dav nrog "profile extrusion" tshwj xeeb. Yas extrusion yog ib tsev neeg loj- tshuab tshuab, cam khwb cia zaj duab xis, ntawv extrusion tag nrho suav. Tab sis profile extrusion tshwj xeeb yog hais txog cov khoom lag luam nrog tus ntoo khaub lig zoo ib yam -section. Lub PVC thav duab nyob ib ncig ntawm koj lub qhov rais, IV tubing ntawm lub tsev kho mob, txawm tias cov quav cab hauv koj McDonald's haus - txiav nws nyob qhov twg raws li nws qhov ntev, thiab tus ntoo khaub lig- seem zoo tib yam. Qhov ntawd yog qhov profile.
Cov khoom uas ua los ntawm profile extrusion tuaj yeem ua tau zoo, zoo li vinyl siding, lossis hollow, xws li haus straws.
Koj ua li cas hollow? Koj yuav tsum muab tus pin lossis mandrel tso rau hauv qhov tuag thiab tshuab cua los ntawm qhov chaw kom cov khoom tsis tawg. Thawj zaug kuv hnov qhov no kuv yuav tsum xav txog nws ib pliag, tab sis tom qab ntawd nws ua rau kev txiav txim siab - yog tias koj tab tom ua ib yam dab tsi hollow thiab koj tsis txhawb nws los ntawm sab hauv, tau kawg nws yuav mus rau hauv qhov tsua.
Ib tus ntsia hlau yuav ua li cas
Lub plawv ntawm lub extruder yog tus ntsia hlau. Funny tshaj plaws yog, rau xws li ib tug loj kev lag luam, qhov tseem ceeb tshaj plaws tivthaiv zoo li ib tug oversized ntoo ntsia hlau.
Cov ntsia hlau tig ntawm qhov kev tswj ceev, feem ntau mus txog 120 rpm, thawb cov yas pellets rau pem hauv ntej ntawm lub thoob. Lub thoob yog rhuab mus rau qhov yuav tsum tau melting kub, uas nyob qhov twg los ntawm 200℃mus rau 275℃nyob ntawm seb dab tsi polymer koj nyob nraum khiav.
Tab sis qhov ntsia hlau tsis yog tsuas yog thawb cov khoom rau pem hauv ntej. Nws yog ib txhij conveying, compressing, melting, thiab homogenizing. Thaum cov yas pellets poob los ntawm lub hopper, lawv yog cov khoom. Raws li cov ntsia hlau thawb lawv mus rau pem hauv ntej, lawv tau raug cua sov los ntawm cov cua sov sab nraud ntawm lub thoob thaum tseem raug txiav ntawm cov ntsia hlau ya dav hlau thiab lub thoob phab ntsa. Thaum lawv ncav cuag qhov kawg, lawv tau molten tag nrho.
Nov yog qee yam uas feem ntau tau saib tsis pom: qhov kub thiab txias feem ntau yog qhov tshwm sim ntawm cov cua sov, thiab qee zaum koj xav tau cua txias ntxiv kom cov yas hauv nws lub qhov rais ua haujlwm.
Cov neeg feem coob xav tias tus extruder tsuas yog siv cov cua sov sab nraud los yaj cov yas. Nyob rau hauv qhov tseeb, shear cua sov tso nyiaj rau ib feem tseem ceeb ntawm lub zog input. Kuv tau saib cov neeg ua haujlwm paub txog kev siv tshuab los ntawm kev ua kom lub tshuab ua kom sov thiab cia shear ua haujlwm ntau dua -txuag hluav taws xob, paub meej, tab sis qhov tseem ceeb tshaj, shear-induced melting tends to be more uniform.

Txog qhov tuag
Qhov tuag yog qhov twg tiag tiag engineering khawv koob tshwm sim. Kuv tsis yog tus kiv cua ntawm cov lus paj, tab sis nws yog qhov tseeb - tuag yog qhov kev xav tau tshaj plaws hauv tag nrho cov kab ke.
Xav txog nws. Molten yas yog cov kua dej. Thaum nws tawm ntawm qhov tuag, nws swells (tuag swell, lawv hu nws). Thaum nws txias, nws shrinks. Qhov sib txawv txias ntawm cov nqi sib txawv, yog li shrinkage tsis zoo ib yam. Txhawm rau kom tau txais cov khoom kawg uas phim cov qauv tsim, cov kab tuag ntws yuav tsum suav rau txhua qhov ntawd.
Thiab ib tug tuag tsis yog ib tug chunk ntawm hlau nrog ib lub qhov txiav los ntawm nws. Qhov sib npaug tuag yog qhov tseem ceeb rau kev tswj kom zoo. "Sib npaug" txhais tau tias ua kom cov dej ntws ntawm qhov sib npaug ntawm qhov sib npaug ntawm tag nrho tus ntoo khaub lig-section. Yog tias cov dej ntws tsis sib xws, koj qhov profile tuaj tawm tuab ntawm ib sab thiab nyias ntawm lwm qhov, lossis ib feem txias ua ntej lwm qhov, thiab tom qab ntawd koj muaj teeb meem.
Kuv paub ib lub Hoobkas uas ua cov profiles complex. Lawv siv peb lub hlis xwb rau kev sim tuag. Tus ntoo khaub lig- ntu muaj xya lossis yim qhov tsis sib xws, phab ntsa nyias tshaj 1 hli, tuab tshaj ze li 8 hli. Nrog rau qhov kev hloov pauv ntawd, kev ua tiav qhov sib npaug yog qhov npau suav phem.
Nws tsis tau ua kom txog thaum nws txias
Cov yas tawm ntawm qhov tuag tseem yog mos. Hom zoo li sov cheese. Koj yuav tsum tau xauv rau hauv cov duab ntawd sai.
Feem ntau txoj hauv kev yog dej txias. Qhov profile mus ncaj nraim los ntawm qhov tuag mus rau hauv lub tank dej. Nyob rau hauv lub tank muaj sizing fixtures uas tuav lub tseem - mos profile nyob rau hauv cov duab thaum nws hardens. Rau cov khoom uas xav tau kev zam nruj dua, koj ntxiv lub tshuab nqus tsev calibration- cov ntaub ntawv muag muag dhau los ntawm lub tshuab ntsuas ntsuas, lub tshuab nqus tsev yog siv rau sab nraud, thiab qhov me me nyob ib puag ncig ib puag ncig nqus cov yas sab nraud tawm tsam phab ntsa calibrator. Nws yog qhov tseem ceeb nruam lub tshuab nqus tsev tsim.
Kev ua kom txias zoo li qhov tho txawv ntawm cov txheej txheem, tab sis muaj ntau txoj hauv kev los ntsia nws. Txias ceev heev thiab qhov kub thiab txias ntawm sab hauv thiab sab nraud tsim kev ntxhov siab sab hauv-warpage tshwm sim tom qab. Txias qeeb heev thiab koj cov nqi tso tawm raug txom nyem, ntxiv rau qhov profile tseem mos thaum lub rub rub nws thiab koj tau ncab.
Dej kub, ntws tus nqi, calibrator ntev, thauj -tawm ceev-txhua yam yuav tsum tau ua hauj lwm.
Lub haul-tawm tswj thiab tswj qhov ceev ntawm qhov profile yog rub tawm ntawm qhov tuag. Qhov ceev yuav tsum phim tus nqi extrusion. nrawm dhau thiab qhov profile stretches nyias. qeeb heev thiab cov khoom piles ntawm qhov tuag tawm. Suab yooj yim. Tuning nws yog tag nrho cov ntsiab lus.
Ob peb lo lus ntawm cov ntaub ntawv
Cov neeg hauv extrusion nyiam tso dag: "Peb extrude yas, tab sis qhov peb poob tiag tiag yog peb cov plaub hau." Tau cov formulation tsis raug thiab txhua yam mus rau sab.
Cov khoom siv xws li polyethylene, polypropylene, polyacetal, acrylic, nylon, polystyrene, PVC, ABS, thiab polycarbonate. Ntawm lwm tus.
Qhov ntawd yog ntau lub npe, tab sis hauv kev tsim khoom tiag tiag koj feem ntau cuam tshuam nrog ib txhais tes.

PVCyog huab tais hauv ntiaj teb profile. Tsis nyob ze thib ob. Lub tsev qhov rais, cov kav dej, cable ducts -nws nyob txhua qhov chaw. Cov ntsiab lus chlorine siab ua rau PVC nyuaj rau ignite thiab txwv kev tso cua sov. Nws yog tus kheej - tua, txhais tau tias nws yuav tsum tsis txhob hlawv thaum koj tshem tawm qhov hluav taws kub. Rau lub tsev cov ntaub ntawv, qhov hluav taws kub kuj yog loj. Ntxiv rau PVC yog pheej yig, corrosion-resistant, thiab koj tuaj yeem ua kom nws nruj lossis hloov tau los ntawm kev ntxiv cov yas yas. Tau kawg nws muaj qhov tsis zoo thiab - qhov rais ua haujlwm nqaim, tsis zoo thermal stability. Koj yuav tsum thauj cov formulation nrog stabilizers los yog nws yuav degrade ua ntej nws txawm tawm ntawm qhov tuag.
PEfeem ntau yog rau cov kav dej. Gas kab siv polyethylene vim nws tiv thaiv corrosion los ntawm ob qho tib si roj thiab ib puag ncig hauv av. Dej mains siv rau tib yam vim li cas, thiab nws pab kom cov dej ntshiab. Kev hloov pauv tau zoo txhais tau tias nws tuaj yeem ua haujlwm hauv av. Thaum tshav kub kub- fused pob qij txha xaus muaj zog dua cov yeeb nkab nws tus kheej.
ABSmuaj kev cuam tshuam zoo heev ua tsaug rau cov tshuaj butadiene, txawm tias qhov kub thiab txias. Tab sis UV raug ua rau microcracking, yog li kev siv sab nraum zoov yuav tsum tau ceev faj.
ASAyog cov khoom siv zoo heev rau kev siv sab nraum zoov, rau cov profiles uas yuav raug tshav ntuj rau lub sijhawm ntev. Ntau tus neeg tsis paub qhov no. Nws yog qhov pib ABS nrog butadiene hloov pauv rau acrylate ester, uas ua rau cov huab cua tsis zoo.
Raws li rau tag nrho lwm yam khoom uas mus rau hauv ib tug formulation: colorants rau tsos, UV stabilizers los tiv thaiv photodegradation, antioxidants qeeb aging, lubricants los txhim kho ntws thiab txo kev sib txhuam, nplaim retardants kom txo cov nplaim taws. Tsis tas li ntawd cov cua sov stabilizers, fillers, tougheners, kev pab cuam... Ib tug paub tab formulation tej zaum yuav muaj ib tug kaum os Cheebtsam, txhua tus dialed nyob rau hauv nws kim heev mus sib hais thiab yuam kev.
Co-extrusion tsim nyog nws ntu
Co-extrusion yog ib txhij extruding ntau txheej ntawm cov khoom. Koj siv ob los yog ntau tshaj extruders pub cov yas sib txawv ntawm tus nqi tswj rau hauv ib lub taub hau tuag, uas muab lawv rau hauv daim ntawv xav tau.
Vim li cas thab?
Vim tias nyob hauv ntau daim ntawv thov tiag - ntiaj teb no, tsis muaj ib qho polymer tuaj yeem ua tau raws li txhua qhov kev xav tau. Hais tias koj xav tau ib qho profile uas cov txheej txheej sab nrauv yuav tsum muaj zog, hnav- tiv taus, thiab zoo- saib, thaum txheej sab hauv yuav tsum mos, elastic, thiab muaj peev xwm tsim tau lub foob. Ib qho khoom siv tsis tuaj yeem ua ob qho tib si. Co-extrusion cia koj khiav ob yam khoom ib zaug, muab lawv tso rau hauv qhov tuag, thiab lawv tawm los ua ib qho kev sib koom ua ke.
Dual durometer co-extrusion fuses ob cov ntaub ntawv nrog qhov sib txawv hardness zones los ntawm tib neeg tuag, muab cov khoom ob qho tib si rigidity thiab yooj. Lub qhov rooj thiab qhov rais seals, cov khoom siv gaskets, ntau yam kev lag luam sealing daim ntawv thov - qhov no tshwm sim.
Lub tsheb qhov rooj ntsaws ruaj ruaj yog ib qho piv txwv classic. Qhov uas clips rau ntawm daim ntawv hlau yog nruj. Qhov chaw uas tiv nrog lub iav los yog lub cev vaj huam sib luag yog mos. Ob yam khoom, ib qho dhau los ntawm kev tuag. Yog tias koj ua lawv cais thiab sim ua ke lawv ua ke, nws yuav raug nqi ntau dua thiab cov ntawv cog lus yuav tsis ntseeg tau.
Nws tau txais complex. Tri-extrusion khiav peb yam khoom siv sib txawv los ntawm ib qho tuag, feem ntau siv rau cov khoom siv kho mob thiab catheters. Kev kho mob tubing muaj qhov yuav tsum tau xav tau- txheej txheej sab hauv yuav tsum tau biocompatible vim nws tiv nrog cov ntshav lossis tshuaj, txheej nruab nrab xav tau lub zog thiab kink tsis kam, txheej txheej txheej yuav tsum tau lubricated rau kev ntxig. Peb lub luag haujlwm, peb cov ntaub ntawv, ib qho kev txhaj tshuaj.
Lub lineup nyob rau hauv pem teb ntau lawm
Ib tug ua tiav profile extrusion kab, txij thaum pib mus rau tiav, zoo li roughly li no:
Cov khoom siv cia / ziab → Extruder → Screen changer → Tuag → Calibration/cooling tank → Haul -tawm → Cutter → Sau / stacking
Twb tau npog lub extruder. Lub vijtsam hloov pauv yog rau kev pom -catches unmelted bits thiab contaminants. Lub haul-tawm yog ob khub ntawm cov menyuam rub lub profile rau pem hauv ntej ntawm qhov ceev tsis tu ncua. Cutters tuaj ntau hom nyob ntawm cov khoom- saws, txiab, ya txiav.
Flexible profiles feem ntau raug mob ntawm cov tshuab coiling tshwj xeeb. Rigid profiles tau sawed los yog sheared rau ntev.
Qee cov khoom lag luam kuj xav tau hauv - kev ua kab. Punching, drilling, thiab slotting yog cov haujlwm zoo ib yam. Inkjet luam ntawv enables batch thiab khoom cim. Hauv -kab xuas nrig ntaus yog txoj kev ua haujlwm zoo dua li offline vim tias qhov profile tseem tab tom txav mus rau hauv kab - lub taub hau punch mus nrog nws, ntaus, thiab nws ua tiav.

Daim ntawv ceev ceev ntawm qhov zoo
Ntau lub chaw tsim khoom tsis tau them nyiaj ntau rau kev teeb tsa kom raug- tsuav yog qhov profile zoo li tau txais, lawv xav tias cov extruder raug hu kom raug.
Uas ntaus tus ntsia hlau rau ntawm lub taub hau. Lub hlwb ntawm ntau cov nroj tsuag yog "yog tias nws thauj khoom, nws zoo," thiab thaum lub tshuab ncav cuag ib hom - ntawm - xeev zoo, tsis muaj leej twg kov nws. Tab sis rau tib yam khoom, optimizing tsis tuaj yeem txiav lub zog siv los ntawm 20% thiab txhim kho qhov sib xws.
Kev tswj qhov kub thiab txias yog txhua yam. Kev tswj qhov kub thiab txias ua kom cov khoom zoo thiab txo cov nqi hluav taws xob tsawg. Thermocoules xav tau kev kuaj xyuas tsis tu ncua. Thaum lub qhov dej yav dhau los- sib npaug tuag pib tsim cov ntaub ntawv tsis sib xws, nws feem ntau vim tias cov thermocouples tsis tswj qhov kub thiab txias kom zoo ntxiv lawm. Thermocouples ya raws lub sijhawm- zaub nyeem 180℃tab sis qhov tseeb yuav yog 195℃-thiab cov teeb meem maj mam nkag mus.
Nws mus qhov twg
Qhov no tsis xav tau kev piav qhia ntau vim tias profiles tsuas yog nyob txhua qhov chaw.
Profile extrusion yog ib qho ntawm ntau tshaj - cov txheej txheem ntim hauv kev tsim cov yas, ua txhua yam los ntawm cov kav dej mus rau qhov rais mus rau kev kho mob tubing.
Kev tsim kho siv feem ntau. Lub qhov rais thav duab, qhov rooj thav duab, sab hauv, lub hauv paus, cov kab hluav taws xob-tag nrho extruded.
Kev kho mob siv qhov tseeb tshaj plaws. Cov hlab ntshav thiab cov catheters yog cov khoom sib xyaw ntawm cov khoom siv yas thiab cov khoom siv ntxiv, uas yuav tsum tau ua tom qab- tsim kom tsis muaj menyuam.
Automotive siv ntau yam. Cov ntsaws ruaj ruaj, luas strips, tubing, hlau hlua tiv thaiv- ib lub tsheb yuav muaj ntau ntau yam extruded profiles.
Cov khoom siv mus tsis hais. Straws, hangers, packing straps, curtain lem ...
Kev xav zaum kawg
Profile extrusion yog qhov siab - ntim cov txheej txheem tsim khoom paub txog kev pov tseg tsawg, tus nqi qis, hloov pauv sai, thiab ntau yam nrog cov ntaub ntawv raw. Nws tseem tuaj yeem ua tiav cov khoom tshwj xeeb xws li nplaim taws ua haujlwm, ua haujlwm ntev, tshuaj lom neeg ua haujlwm, thiab kub ua haujlwm.
Txhua yam muaj tseeb raws li phau ntawv qhia cov ntsiab lus mus. Tab sis dab tsi tiag tiag muab cov txheej txheem no nws lub zog nyob twj ywm, kuv xav tias, yog qhov txuas ntxiv. Txhaj tshuaj molding ua haujlwm nyob rau hauv lub voj voog - pwm qhib, pwm kaw, muaj sijhawm tuag ntawm kev txhaj tshuaj. Extrusion tsuas yog khaws cov khoom siv tawm. Koj tuaj yeem khiav nws 24 teev ncaj yog tias koj xav tau. Qhov txiaj ntsig txuas ntxiv ntawm tus nqi no yuav luag tawg thaum koj hais lus siab - ntim ntau lawm.
Tau kawg muaj kev txwv. Koj tsuas tuaj yeem ua tus ntoo khaub lig tsis tu ncua - cov khoom seem. Precision yog qis dua kev txhaj tshuaj molding. Complex 3D geometries yog tawm ntawm lo lus nug. Tab sis hauv nws lub log tsheb, tsis muaj dab tsi los ze.
Cov cuab yeej technology thiab cov khoom siv tau nce ntxiv kom rov ua kom cov toj roob hauv pes ntawm profile extrusion. Kev sib koom ua ke ntawm cov qauv tsim thiab simulation software, kev txhim kho siab -kev ua tau zoo polymers-txhua qhov nthuav dav qhov ua tau raws li cov qauv tshiab thiab ntau yam kev ua haujlwm.
Profiles uas tsis tuaj yeem ua tau kaum xyoo dhau los tuaj yeem ua tam sim no. Parameters uas siv los nyob ntawm tag nrho cov qub tub rog tswv 'intuition tam sim no tau simulated hauv software. Kev lag luam txuas ntxiv mus tom ntej. Cov hauv paus ntsiab lus tsis tau hloov pauv ntau hauv ib puas xyoo, tab sis qhov ntau ntawm qhov koj tuaj yeem rub tawm yuav loj tuaj.