Sprue khoom (khiav sprue) lo rau pwm thiab kev daws teeb meem

Dec 13, 2025

Tso lus

injection molding

Thaum lub sij hawmtxheej txheem txhaj tshuaj, qhov tshwm sim uas cov khoom siv nozzle (khiav sib sau ua ke) sticks hauv pwm khiav tom qab lub pwm qhib thiab tsis tuaj yeem tev tawm yog hu ua dej txhaj tshuaj.Cov khoom siv lub qhov ncauj sticks rau pwm. Qhov laj thawj tseem ceeb yog vim li cas cov khoom siv nozzle sticks rau cov pwm yog tias qhov apertures ntawm lub tshuab txhaj tshuaj nozzle thiab sprue bushing (tseem ceeb bushing) tsis sib xws.Burrs (undercuts) yog generated thiab tsis tuaj yeem tshem tawm ntawm cov pwm smoothly. Qhov ua rau thiab kev daws teeb meem rau qhov tshwm sim no tau qhia hauv cov lus hauv qab no.

 

Yog vim li cas thiab kev daws teeb meem rau cov khoom nozzle los lo rau pwm

 

Ua rau Analysis Txoj kev daws teeb meem
① Cov kua nplaum ntau dhau los yog tsis tshua muaj siab ① Txo cov kua nplaum los yog tsis tshua muaj siab
② Txheej kub kub heev ② Tsawg txheej txheej kub
③ Lub ntsiab khiav nkag nkag thiab sprue bushing tsis haum zoo ③ Txhim kho qhov xwm txheej ntawm lub ntsiab nkag nkag thiab sprue bushing
④ Cov neeg khiav dej num tseem ceeb tsis du lossis muaj cov ces kaum ntse ④ Polish lub ntsiab khiav los yog txhim kho cov ces kaum ntse
⑤ Main khiav inlet txoj kab uas hla me dua nozzle txoj kab uas hla ⑤ Txhim kho lub ntsiab khiav hauv qhov taub
⑥ Main khiav inlet sib npaug R me dua lub taub hau R ⑥ Txhim kho lub ntsiab khiav hauv qhov sib npaug R
⑦ Lub qhov tseem ceeb ntawm qhov chaw khiav tsis sib haum nrog lub taub hau ⑦ Kho lub qhov taub qhov nruab nrab kom ua kom haum rau tib txoj kab
⑧ Khiav sab nrauv puas los yog sprue taub hau tsis du ⑧ Kho pwm, kho qhov chaw puas, ntxuav lub taub hau (tiv thaiv kev ua burrs)
⑨ Main khiav tsis rub nuv ⑨ Ntxiv rub nuv ntawm qhov kawg ntawm sprue los yog Z-puab rub nuv
⑩ Lub ntsiab khiav qhov ntev loj dhau los yog lub sijhawm txias tsis txaus ⑩ Txo qhov loj ntawm qhov khiav los yog ncua sij hawm txias
⑪ Lub ntsiab khiav demolding lub kaum sab xis me dhau ⑪ Nce lub ntsiab khiav demolding lub kaum sab xis

 

Pwm qhib nyuaj thiab kev daws teeb meem

 

Thaum lub sij hawm txhaj tshuaj molding txheej txheem, yog tias muaj ntau lub zog clamping, pwm core misalignment, coj ncej coj, los yog pwm nyob rau hauv siab -siab clamping lub xeev ntev, ua rau pwm deformation thiab "tom qab quab yuam", lub pwm yuav qhib tsis tau. Qhov tshwm sim no suav nrog hu ua pwm qhib nyuaj. Thaum cov yas loj dua, cov pwm nrog cov kab noj hniav sib sib zog nqus, lossis cov tshuab txhaj tshuaj molding siv lub tshuab hloov clamping, cov saum toj no - hais txog qhov tsis zoo yuav tshwm sim ntau dua. Qhov ua rau thiab kev daws teeb meem rau qhov tshwm sim no tau qhia hauv cov lus hauv qab no.

 

Yog vim li cas rau cov teeb meem hauv pwm ua thiab lawv cov kev daws teeb meem.

 

Ua rau Analysis Txoj kev daws teeb meem
① Pwm kab noj hniav quab yuam ua rau deformation ntawm pwm, ua rau "tom" ① Txhim kho cov pwm, txo lub zog clamping
② Cov lus qhia / cov lus qhia xoob dhau, clamping quab yuam siab dhau ② Ntxuav/lubricate cov lus qhia/cov lus qhia, hloov bushings
③ Txias lub sij hawm ntev dhau, ua rau muaj kev kub siab kaw lub xeev ③ Txo lub sijhawm txias (nce siab)
④ Ib ntu ntu ntu xoob, pwm tuab tsis sib haum ④ Reinforce xoob pwm, kho pwm thickness ntsia hlau
⑤ Ejection mechanism kev sib txhuam tsis txaus ⑤ Txhim kho lub zog tawm los yog hloov nrog lub tshuab ejection loj dua
⑥ Pwm tso qhov system thaiv, ua rau "tsis zoo siab" ⑥ Ntxuav cov qhov tso tawm / qhov cua hauv cov pwm kab noj hniav lossis qhov chaw sib cais (lossis los ntawm cov pa tawm)
⑦ Tsis sib luag rub quab yuam los ntawm peb daim hlau (lub zog tsis txaus) ⑦ Ua kom lub zog ntawm rub hooks

Lus Cim: Rau kev txhaj tshuaj molding tshuab nrog tus qauv toggle - hom clamping mechanism, pwm qhib quab yuam tsuas yog ncav cuag li 80% ntawm cov ntsuas clamping quab yuam.

 

Cua nkag los ntawm kub khiav tshuab thiab nws cov kev daws teeb meem

Thaum siv lub tshuab hluav taws xob kub nrog lub qhov rooj valve rau kev txhaj tshuaj molding, yog tias siv semi-kub, semi- txias khiav system, raws li qhia hauv daim duab, huab cua hauv cov neeg khiav dej txias yuav tsum muaj peev xwm ua tau zoo thiab tshem tawm tag nrho raws li cov yaj ntws los ntawm rab koob valve nozzle mus rau hauv qhov txias khiav. Txwv tsis pub, cov pa roj yuav raug daig los ntawm cov yaj uas ntws tawm ntawm lub rooj vag ntawm rab koob, ua rau muaj cov npuas hauv cov khoom molded.

injection molding

Nyob rau hauv kub khiav pwm siv rau kev khiav hauj lwm ntev, vim qhov kub thiab txias los yog tsub zuj zuj ntawm cov khoom volatile, qhov cua txias khiav txuas nrog cov kub khiav tuaj yeem cuam tshuam. Yog tias tus neeg khiav dej txias nws tus kheej tsis muaj qhov ua kom zoo lossis muaj qhov ua haujlwm tsis zoo, nws tuaj yeem ua rau cov pa nkag mus rau hauv pwm kab noj hniav thiab ua rau npuas hauv cov khoom pwm.

 

Ntev ntev molding voj voog thiab kev daws teeb meem.

 

Hauv kev txhaj tshuaj molding txheej txheem, cov laj thawj rau qhov txawv txav mus ntev molding cycles thiab cov kev ntsuas sib xws yog raws li hauv qab no:
① Kev kub siab yas, ua rau lub sijhawm txias txias rau cov khoom. Yog li ntawd, qhov kub ntawm lub thoob yuav tsum tau txo qis, cov ntsia hlau ceev los yog rov qab siab yuav tsum tau txo, thiab qhov kub ntawm txhua seem ntawm lub thoob yuav tsum tau kho kom zoo.
② Kub pwm kub, ua rau lub sij hawm ntev yaj solidification. Txawm li cas los xij, pwm kub kub feem ntau yog qhov zoo rau molding thiab ua tiav cov khoom zoo; Yog li ntawd, qhov txias ntawm cov dej channel yuav tsum tau kho tshwj xeeb.
③ Lub sijhawm molding tsis ruaj khov. Tsis siv neeg lossis semi- tsis siv neeg molding yuav tsum siv.
④ Cov cua kub tsis txaus ntawm lub thoob, uas ua rau lub sij hawm plasticization ntev heev. Lub tshuab uas muaj lub peev xwm loj dua yuav tsum tau siv, los yog preheating ntawm cov khoom siv yas yuav tsum tau txhim kho.
⑤ Nozzle drooling. Lub tshuab txhaj tshuaj tsis ruaj khov thaum lub sijhawm txhaj tshuaj molding txheej txheem. Qhov kub ntawm lub thoob thiab lub nozzle yuav tsum tau tswj, los yog yuav tsum tau siv tus kheej -lock nozzle.
⑥ Cov phab ntsa thickness ntawm cov yas yog tuab heev, ua rau lub sij hawm ntev heev. Cov qauv pwm yuav tsum tau txhim kho kom txo tau cov phab ntsa tuab ntawm cov yas.
⑦ Txo qhov kev faib ua feem ntawm cov ntxhia hauv cov khoom siv, cov thermal conductivity tsawg, thiab cov crystallization tsawg ntawm cov khoom tuaj yeem ua rau lub sijhawm molding ntev heev.

injection molding

⑧ Lwm yam kev ntsuas zoo los txo lub voj voog molding: siv cov pwm kub khiav kom luv lub voj voog molding. Raws li pom nyob rau hauv daim duab, rau ib tug loj ib feem, CAE pwm flow tsom tau ua. Tus thawj pwm siv cov pa khiav, yuav tsum tau 51.28s; Tom qab hloov mus rau qhov kub khiav pwm, lub voj voog molding tsuas yog xav tau 25.63s.

 

Lwm yam tshwm sim txawv txav hauv kev txhaj tshuaj molding thiab lawv cov kev daws teeb meem.

 

Thaum lub sij hawm txhaj tshuaj molding txheej txheem, vim muaj kev cuam tshuam ntawm ntau yam xws li yas raw cov ntaub ntawv, pwm, txhaj tshuaj molding tshuab, molding txheej txheem, kev khiav hauj lwm txoj kev, Rhiav ib puag ncig, thiab kev tswj ntau lawm, muaj ntau yam txawv txav tshwm sim. Ntxiv rau qhov tsis xws luag, lwm yam tshwm sim txawv txav xws li cov ncej tawg thiab cov yas ntau dhau kuj tuaj yeem tshwm sim. Cov laj thawj thiab kev daws teeb meem rau cov xwm txheej txawv txav no tau qhia hauv cov lus hauv qab no.

 

Lwm yam tshwm sim txawv txav thiab lawv cov kev daws teeb meem

 

Phenomenon tsis zoo Ua rau Analysis Txoj kev daws teeb meem
Flash ① Txhaj tshuaj los yog tuav lub siab ntau dhau ② Tsis txaus pwm clamping quab yuam los yog lub teeb tsis sib xws ntawm qhov sib cais, lub sij hawm txias tsis txaus ③ Cov khoom siv roj hmab muag muag heev ① Txo kev txhaj tshuaj los yog tuav lub siab ② Ua kom cov pwm clamping quab yuam, polish (nqus) pwm ③ Tsawg yaj kub, txo cov khoom me me.
Ntau kab Pwm (tsawg- qhov kub thiab txias) cov khoom siv nrog khawb, kev ua haujlwm ntxhib / cov pa paug tsis zoo / cov khoom hnav tsis zoo muaj qhov khoob me me Tshawb xyuas pwm thiab hloov / kho cov khoom sab hauv nrog cov xwm txheej hnav
Hlawv cim Pwm (tsawg- qhov kub thiab txias) muaj cov ntsiab lus convex, paj, khawb, qhov grooves, thiab pwm puas, thiab lwm yam. Kho pwm, txhim kho qhov chaw nrog khawb / qhov rau ntawm pwm, tiv thaiv kev hnav thiab cov cim siab
Sab saum toj koob convex defect Internal 过长 los yog protruding ntau heev Shorten sab saum toj koob ntev los yog kho tus nqi
Sab saum toj koob Cov koob sab saum toj muaj cov khoom siv sab hauv, cov koob sab saum toj lub cev ntev tsis txaus lossis lub taub hau saum lub taub hau nyias dhau Ua kom cov koob sab saum toj ntawm cov khoom, nce lub koob ntev ntev lossis ua kom lub taub hau tuab
Sab saum toj koob perforation Sab saum toj koob rear daim npav sab saum toj koob lub qhov, uas ua rau "kawg koob" Tshawb xyuas / hloov lub koob sab saum toj, huv si sab laug hauv nruab nrab ntawm lub rooj zaum saum lub koob, ntxiv lub rooj zaum saum lub koob (tiv thaiv hnav)
Sab saum toj koob Sab saum toj koob qhov phab ntsa, yaj nkag mus rau sab hauv Nthuav cov koob txhaj tshuaj saum toj kawg nkaus, nce ntau lawm khiav, txo cov koob kub saum toj kawg nkaus, txo ejection ceev, txo txhaj tshuaj siab / txo cov koob lub rooj zaum siab
Ejector pin marks Ejector tus pin tiaj tus, ejector tus pin ntau dhau, ejector tus pin txoj kab uas hla loj dhau, ejection ceev dhau, ejection ncua ntev dhau Ntau ejector pins, ntau lawm hauv ejector tus pin mechanism, txo ejector tus pin txoj kab uas hla, txo ejection ceev, txo ejection ncua / tuav ceev
Pwm sticking rau sab ruaj Tsis tshua muaj zog quab yuam siab heev, txias luv luv (shrinkage), khoom zoo, siab dhau heev lawm Cov khoom siv ntau dua / tsawg dua, siv tus neeg sawv cev tso tawm / nce pwm kub, txo kev txhaj tshuaj thiab tuav lub zog, nce siab
Tsab ntawv thaiv (niam ntawv thaiv) nto Letter / alphabet block (niam ntawv thaiv) kev taw qhia rov qab thaum tsab ntawv thaiv zawv zawg Kho tsab ntawv thaiv kev teeb tsa lossis ntxiv qhov chaw tus pin