Yas Yeeb Nkab Extrusion

Sep 16, 2025

Tso lus

 

Yas yeeb nkab Extrusion sawv cev rau ib qho ntawm cov txheej txheem tseem ceeb tshaj plaws hauv kev lag luam niaj hnub no uas pab txhua yam ntawm cov kav dej uas muaj cov ntawv thov kev lag luam. Cov txheej txheem ntse no, uas hloov cov khoom nyoos polymer los ntawm kev ua tiav cov cuab yeej siv kho tshuab thiab cua sov, tau hloov kho cov txheej txheem kev loj hlob thoob ntiaj teb.

 

Nrog rau ntiaj teb yas yeeb nkab tau tshaj 18 lab Metric tons thiab kev nkag siab cov kab ke yas ntxiv rau cov engineers, cov kws tsim khoom, thiab cov kws tshaj lij kev lag luam, thiab cov kws tshawb fawb, thiab cov kws tshawb fawb, thiab cov kws tshawb fawb, thiab kev lag luam kev lag luam, thiab cov kws tshawb fawb, thiab kev lag luam cov kws tshawb fawb.

Plastic pipe extrusion
 

Ntau lawm kab ntev

30-60 Metres

Niaj hnub extrusion kab feem ntau ntsuas ntawm 30 txog 60 meters ntev

Yeeb Nkab Txoj Kab Uas

16 hli-2400mm

Extrusion tshuab tuaj yeem tsim kav kav dej los ntawm 16 hli rau 2400 hli hauv lub taub

Qhov seem ntev

± 0.1mm

Txhua tus sib xyaw ua ke tswj hwm kev thev taus, feem ntau tsis pub dhau ± 0.1mm

 

Cov cuab yeej ua tiav ua ke ua ke

 

Cov txheej txheem yeeb nkab yas Extrusion cov txheej txheem kev sib dhos rau cov cuab yeej sib dhos kom sib dhos uas ua haujlwm nrog kev ua kom zoo tshaj plaws. Lub kaw lus ua tiav muaj rau thawj lub Cheebtsam ua haujlwm hauv synchronized kev sib haum xeeb.

Extruder Chav

Lub plawv ntawm cov yeeb nkab yas cov kab ntawv extruster nws tus kheej, feem ntau yog ib qho los yog ntxaib}} Txoj kev sib piv ntawm 24: 1 txog 36: 1.

Zauv Zauv Kub: 160 Qib rau 220 Qib

Ntsia Hlau Ceev: 10 txog 120 RPM

4 mus rau 8 thaj chaw ua cua sov nrog ± 1℃tswj

Extruder Unit

Tuag Lub Taub Hau Tus Qauv

Cov qauv tuag sawv cev sawv cev sawv cev pom tias qhov tseem ceeb tshaj plaws hauv kev txiav txim siab cov yeeb nkab zoo thiab qhov tseeb raug thiab qhov raug. Niaj hnub nim cov txiv neej niaj hnub ua hauj lwm zoo muab cov khoom siv mirral elrel.

Compression Piv: 10: 1 txog 20: 1

Kev khiav hauj lwm siab: 200 txog 400 bar

Tswj qhov kub thiab txias: ± 2℃ntawm kev teeb tsa

Die Head Structure

Calibration & sizing

Lub Appration Apparatus txiav txim siab zaum kawg thaum cov khoom tseem nyob hauv ib nrab {{0} Lub xeev yas. Lub tshuab nqus hluav taws xob yog feem ntau hom.

Nqus Plua Plav Siab: 0.4 mus rau 0.8 bar

Dej Txias: 15 Qib rau 25 degree

3 txog 5 lub tshuab nqus tsev

Calibration & Sizing

Cov Tshuab Cua Txias

Cov apparing txias txuas ntxiv ntsuas qhov ntsuas kub nyob hauv chav ntsuas hluav taws xob, ntsuas cov yeeb nkab rau qib, feem ntau qis dua 40 degree.

Qhov ntev: 6 txog 12 meters
Dej Flow Cov Nqi: Txog li 500 ML / teev
Kab ceev: 0.5 txog 15 m / feeb

Cooling Systems

Haul - tawm chav

Tus hau - tawm cov apparatus muab lub zog rub tawm tsim nyog los kos cov yeeb nkab los ntawm tag nrho cov kab sib txawv.

Rub cov rog: 5,000n rau 100,000n

Hu Rau Siab: 2 Rau 6 bar

Cov neeg ceev ceev: ± 0.1%

Haul-off Unit

 

Die Head Structure and Design Principles

Tuag lub taub hau qauv thiab tsim cov ntsiab cai

Cov qauv tuag sawv cev sawv cev sawv cev pom tias qhov tseem ceeb tshaj plaws hauv kev txiav txim siab cov yeeb nkab zoo thiab qhov tseeb raug thiab qhov raug. Cov hau kev tuag niaj hnub ua haujlwm tau muab cov qauv tsim qauv uas faib cov molten polymer uncepororm, tshem tawm weld kab uas tuaj yeem ua rau muaj kev ncaj ncees.

 

Lub compression piv nyob rau hauv tus tuag feem ntau yog li ntawm 10: 1 txog 20: 1, tsim cov khoom siv tsim nyog {}

 

Tswj kub nyob hauv lub taub hau tuag nyob hauv lub taub hau tuag Cov sib txawv tuag, uas txiav txim siab phab ntsa tuab, yuav tsum tau kho kom them rau cov khoom shrinkage cov nqi uas feem ntau ntawm 1.5% rau cov thermoplastics.

 

Cov neeg siv hluav taws xob siab dhau los siv tshuab hluav taws xob hnyav

 

Lub thev naus laus zis ntawm cov tub ntxhais hluas niaj hnub no cov tsom iav ua haujlwm hauv lwm qhov siab - Tech Industries. Ib yam li dab tsi tso cai rau digital cov qauv thiab xa lub taub hau txaus los ua kom muaj Laminar ntws tawm thiab txo cov siab ua kom muaj peev xwm ua rau muaj qhov tsis sib haum.

Kev ntsuas tshuaj thiab cov khoom siv sizing

Lub calibration apparatus, muab tso rau tam sim ntawd tom qab tuag lub taub hau, txiav txim siab cov yeeb nkab kawg thaum cov khoom nyob hauv ib ntu semi- Lub xeev yas. Lub tshuab nqus hluav taws xob muaj kev tso tsheb hlau luam, siv cov hom tsis zoo ntawm 0.4 mus rau 0.8 bar kom kos cov yeeb nkab kub tawm tsam lub tes tsho.

 

Cov tes tsho no, feem ntau tsim los ntawm cov hlau stainless lossis tooj dag, tswj qhov seem

 

Kev ntsuas hluav taws xob rau cov yeeb nkab cov yeeb nkab kom tau txais kev ceev faj kom ua tau zoo ntawm cov txias tus nqi thiab qhov ruaj khov sab ruaj khov. Kev ua kom txias heev tuaj yeem ua rau muaj kev cuam tshuam ntev ntev ua rau ntev-} sij hawm hloov chaw, thaum tsis txaus ua rau cov yeeb nkab deformation.

 

Niaj hnub nimno calibration tank ua hauj lwm ntau thaj chaw - ib txwm 3 txog 5-nrog kev ntxhov siab zuj zus thaum tswj kev tswj hwm ib qho seem. Lub calibration ntev feem ntau sib npaug 10 txog 20 zaus ntawm cov kab yeeb nkab, kom ua tiav cov kev ruaj khov ua ntej nkag mus tom ntej.

Calibration and Sizing Equipment
Advanced Cooling Systems

Kev Ua Kom Txias Tshuab

Cov apparing txias txuas ntxiv ntsuas qhov ntsuas kub nyob hauv chav ntsuas hluav taws xob, ntsuas cov yeeb nkab rau qib, feem ntau qis dua 40 degree. Muaj cov tshuab ua dej txias ua haujlwm txau hlau luam lossis dej phwj dej txuas ntxiv 6 txog 12 meters, nrog dej kub tswj tsis pub dhau ± 1 degree.

 

Cov dej ntws tau tuaj yeem ncav cuag 500 teev cubic metre ib teev

 

Cua txias ua hluav taws xob ncaj ncees ntau lawm cov nqi, nrog kab kev nrawm nrawm xws li 0.5 txog 15 metres ib feeb nyob ntawm cov kab ntsig thiab phab ntsa tuab. Tus txheej txheem cua txias yuav tsum tau nyiaj rau cov khoom siv hluav taws xob polymer cov cua sov, tshwj xeeb yog thermal conductivity tseem ceeb uas tau los ntawm 0.15 txog 0.45 W / MIN Cov ntaub ntawv yeeb yam.

 

Qhov no tseem tsis tau thermal conductivity yuav tsum tau txuas ntxiv cov cheeb tsam, tshwj xeeb yog lub sij hawm txias rau lub sij hawm txias ua raws li cov xwm txheej square kev sib raug zoo nrog phab ntsa tuab.

"Qhov kev ua kom zoo dua ntawm cov khoom txias hauv cov yeeb nkab yas ntxiv nrog kev ua kom tsawg dua nrog kev ua kom tsawg dua li ntawm 0.5% thaum siv tau zoo"

Schmidt, K. li al.

Qhov kev kawm tau ntawm cov tshuab cua txias niaj hnub hauv datacenter interconnect technology, qhov twg meej thermal kev tswj hwm thiab kev ntseeg tau. Ib yam li cov ntaub ntawv tawm tswv yim yuav tsum tau ua haujlwm yooj yim, yas yeeb ntxig rau cov khoom txias kom ua tiav cov khoom lag luam zoo ib yam.

 

Kev Sib Tham Txog Kev Siv Tshuab & Automation

 

Niaj hnub niaj hnub yas yeeb tshuaj extrusion nkag rau in6- ntug tshuab los xyuas kom meej qhov tseeb, thiab zoo nyob thoob plaws txhua qib.

Haul-off Unit Technology

 

Haul - tawm ntawm chav tsev thev naus laus zis

 

Tus hau - tawm cov apparatus muab lub zog rub tawm tsim nyog los kos cov yeeb nkab los ntawm tag nrho cov kab sib txawv. Niaj hnub nimno - tawm ntawm cov khoom siv lossis rho tawm cov kab ntsig los ntawm 5,000n rau cov tub kab ntsig me me mus rau ntau dua 100,000n rau cov khoom sib tw loj loj.

 

Lub siab sib tiv tauj yuav tsum ua tib zoo tswj}}} feem ntau 2 txog 6 bar - kom tau tuav cov yeeb nkab txaus.

 

Synchronization ceev sawv cev rau lub qhov tseem ceeb ntawm Haul - tawm cov haujlwm, nrog kev hloov ceev ntau yam rau cov phab ntsa tuab. Advanced Systems Comporporate kaw {} Voj tswj kev tswj siv laser velocity sensors uas tswj kom ceev ceev rau hauv ± 0.1%.

 

Tus hau -}} chav tsev yuav tsum tau kho hluav taws xob (raws li cov kav dej txias, yuav tsum tau hloov kho kom nrawm nrawm rau kom tswj tau cov kev pom zoo.

Cutting Equipment and Automation

 

TEJ KHOOM SIV THIAB KEV LAG LUAM

 

Qhov txiav cov apparatus sawv cev rau theem kawg hauv cov txheej txheem yeeb nkab yas hauv cov txheej txheem sib txawv, hloov ua ntej hloov mus rau hauv ntev. Niaj hnub sib txiav cov tshuab ua haujlwm rau lub ntiaj teb saws rau txoj kab uas hla loj, ua tiav ib feeb nrog ntev tshaj ntawm ± 2mm.

 

Cov khoom txiav txiav yuav tsum synchronize nrog kab nrawm, ntiav ya cov yeeb nkab uas phim cov kev txiav kom ua kom pom kev sib txuas.

 

Automated tej tshuab tam sim no ua ke nrog kev tswj hwm software ntau heev, ua rau kev ua kom zoo dua kom txo qis tsawg dua li 1% ntawm tag nrho cov khoom lag luam. Cov kab ke no, kev khiav siab zoo sib xws rau kev sib txuas lus hauv kev sib txuas lus, tswj xyuas ntau yam kev tsim tawm los ua kom zoo tag nrho cov kev ua haujlwm.

 

Kuaj xyuas online

Laser micrometers thiab ultrasonic phab ntsa tuab gauges ntes cov khoom me me li 0.1mm, tsim ntau dua 10,000 kev ntsuas ib feeb.

Kev Kuaj Neeg Kho Tshuab

Tensile Develfease (feem ntau 19 {{{}}}} hydrostatic lub zog kuaj ntawm nias txog li 20 bar.

Tshuaj Kuj

Kev kuaj kom ntseeg tau cov kav dej PIPES ntsib - kev cai rau kev ib puag ncig ntau yam thiab kev ua haujlwm.

 

Seem ruaj khov

Kev ntsuam xyuas paub tseeb shrinkage tseem nyob rau hauv kev txwv tshwj xeeb tshaj 24-teev txias lub sijhawm nyob rau ntau qhov kev mob siab.

 
 

Kev tswj kom zoo thiab qauv ua raws

Tswjhwm zoo hauv cov yeeb nkab yas extrusion enccompasses ob qho tib si online thiab cov txheej txheem sim ua haujlwm offline. Kev ntsuas ntsuas online ua haujlwm laser micrometers, ultrasonic phab ntsa tuab gauges, thiab kho qhov muag deg ntawm qhov tsis taus li 0.1 hli. Cov kab ke no tsim ntau dua 10,000 kev ntsuas ib feeb, tsim cov ntaub ntawv zoo rau txhua qhov kev tsim khoom.

 

Offline testing includes mechanical property evaluation such as tensile strength (typically 19-25 MPa for PVC pipes), impact resistance, and long-term hydrostatic strength testing at pressures up to 20 bar. Tshuaj lom neeg Kev sim ua kom cov kav dej ua kom tau raws li daim ntawv thov kom paub meej meej, thaum muaj kev ntsuas qhov tsis raws cai los ntawm kev txwv ntawm 24-teev txias.

 

Cov Qauv Thoob Ntiaj Teb

Yog {0 4427
Polyethylene kav rau Watersupply
Yog {0 1452-2
Yas roj rau roj

ASTM D1785

Pvc Kav Rau Kev Siv Siab

ASTM F441

PE PIPES RAU DEJ

 

Ib puag ncig kev txiav txim siab thiab muaj kev ruaj khov

 

Ib puag ncig kev nco qab nyob rau hauv yas yeeb extrusion tau coj mus rau cov thev naus laus zis tseem ceeb thaum tswj cov khoom zoo.

 

Environmental Considerations and Sustainability
 

Ib puag ncig nco qab nyob rau hauv yas yeeb extrusion tau coj mus rau cov thev naus laus zis tseem ceeb. Niaj hnub no cov chaw ua tiav cov khoom siv siv nyiaj ntau tshaj 99% los ntawm cov khoom siv inline ntawm Startup thiab cov khoom txiav txiav.

Kev siv zog siv tau tsawg dua 30% dhau ntawm xyoo dhau los los ntawm kev txhim kho cua sov txhim kho, nrog cov khoom siv niaj hnub los siv 0.25 rau 0.35 kilogram ntawm cov khoom siv ua tiav.

 

Kev siv ntawm kaw - loop txias tshuab txo cov dej kom sov li ntawm 95%, thaum tshav kub rov qab los yog cua sov lossis cua sov ntawm cov khoom siv raw.

 

Cov kev ntsuas cov kev ntsuas kom haum rau kev lag luam kev lag luam ncig, uas yog cov neeg siv khoom siv tau ntev txog 40% ntawm raw khoom hauv qee cov kab ntawv.

 

99%

Cov Khoom Siv Siv Kev Siv Los Ntawm Inline Recycling

30%

Txo hauv kev siv hluav taws xob hauv lub xyoo dhau los

95%

Txo hauv kev noj dej nrog kaw - voj tshuab

40%

Post - Cov Neeg Siv Khoom Siv Rov Siv Cov Yeeb Nkab Tshaj Plaws Hauv Cov Yeeb Nkab