Dav hlau qauv (serpentine qauv) thiab lawv cov kev daws teeb meem

Dec 01, 2025

Tso lus

 

Thaum txhaj tshuaj molding, yog tias qhov kev txhaj tshuaj ntawm cov yaj ntawm lub rooj vag nrawm dhau, tus nab - zoo li tus qauv yuav raug tsim nyob rau saum npoo ntawm cov yas (hauv pem hauv ntej ntawm lub rooj vag sab). Lub hauv paus ntsiab lus tsim muaj nyob rau hauv daim duab 3-48, thiab cov khoom tshwj xeeb tau pom hauv daim duab 3-49.

 

info-726-260

info-881-213

 

Nab-zoo li cov qauv feem ntau tshwm thaum pwm siv lub rooj vag sab. Thaum molten yas ntws los ntawm kev kub ceev los ntawm qhov chaw nqaim xws li nozzles, cov neeg khiav dej num, thiab cov rooj vag, nws mam li nkag mus rau qhov chaw dav dav. Cov khoom molten ces meanders raws cov kev taw qhia ntws zoo li ib tug nab, sai txias thaum sib cuag nrog pwm nto, raws li qhia nyob rau hauv daim duab 3-51. Vim tias feem ntawm cov khoom siv no tsis tuaj yeem ua haujlwm zoo nrog cov resin tom qab nkag mus rau hauv cov kab noj hniav, cov qauv pom ntawm cov khoom. Nyob rau hauv tej yam kev mob, lub yaj pib tawm lub nozzle ntawm ib tug kuj tsis tshua muaj kub. Ua ntej hu rau cov kab noj hniav saum npoo, cov yaj viscosity siab heev, ua rau tus nab -zoo li ntws. Raws li qhov kub kub tseem nkag mus rau hauv cov kab noj hniav, qhov pib yaj yog yuam kom tob rau hauv pwm, tawm hauv cov qauv zoo li nab.

 

info-579-206

Daim duab 3-51 Snake qauv tsim los ntawm Moldflow simulation

 

Qhov ua rau thiab kev daws teeb meem rau cov qauv serpentine ntawm cov khoom yas yog qhia hauv cov lus hauv qab no.

Original Analysis (Common Faults) Kev daws / Kho Txoj Kev
① Txoj hauj lwm nozzle tsis raug (ntsuas ncaj qha rau ntawm qhov ntsuas kub tswj) ① Hloov txoj haujlwm nozzle (tsav mus rau sab)
② Cov khoom kub siab dhau lawm ② Txo qhov kub ntawm lub thoob
③ Kev txhaj tshuaj nrawm dhau lawm (ze ntawm lub rooj vag cheeb tsam) ③ Txo qhov kev txhaj tshuaj nrawm (tshwj xeeb ze ntawm lub rooj vag)
④ Lub rooj vag loj me dhau los yog tsis sib xws (sab rooj vag) ④ Loj lub rooj vag lossis hloov mus rau lub rooj vag hauv nruab nrab (lossis ua kom zoo dua lub rooj vag ze rau thaj tsam phab ntsa tuab)
⑤ Plastic flowability (FPI siab dhau) ⑤ Siv cov yas uas muaj dej ntws zoo dua

 

Tsov kab txaij thiab kev daws teeb meem

Tsov - daim tawv nqaij qauv yog hais txog qhov tsis xws luag zoo li tsov tawv nqaij ntawm cov yas loj. Nws feem ntau pom nyob rau ntawm dashboards, bumpers, qhov rooj vaj huam sib luag, thiab lwm yam loj - thaj chaw yas uas muaj txoj hauv kev ntev. Nws tseem hu ua tsov- daim tawv nqaij, raws li pom hauv daim duab 3-53.

Cov ntaub ntawv polymer yog viscoelastic; lawv shrink nyob rau hauv siab thiab nthuav raws li regaining lawv thawj ntim thaum lub siab tso tawm. Thaum cov polymer yaj yog extruded los ntawm ib tug tuag, tus ntoo khaub lig-sectional cheeb tsam ntawm lub extrudate yog loj tshaj qhov tuag tawm cross-sectional cheeb tsam.

Qhov no tshwm sim yog hu ua tuag expansion. Nws tau pom thawj zaug los ntawm American biologist Barus hauv 1893, yog li lub npe "Barus effect."

Thaum lub sij hawm txhaj tshuaj molding, thaum cov yas yaj dhau los ntawm lub rooj vag me me, nws ntsib qhov kev tiv thaiv tseem ceeb ntawm lub rooj vag, ua rau muaj qhov ntim loj hauv cov neeg khiav dej num. Thaum nws dhau los ntawm lub rooj vag, nws tam sim ntawd nthuav, ua rau muaj kev nthuav dav dhia raws cov yaj ntws pem hauv ntej, uas tshwm sim raws li Tsov - daim tawv nqaij qauv.

 

info-655-254

Tsov- daim tawv nqaij qauv ntawm cov yas (Daim duab 3-53)

 

Ib yam li ntawd, thaum lub sij hawm yaj ntws, yog hais tias ib feem yog nyias, cov kab noj hniav clearance yog me me, thiab cov pwm kub tsis tshua muaj, cov qauv ntawm cov khoom yuav ua rau muaj teeb meem txaus los yog txoj kev khiav ntev heev, ua rau muaj zog tiv thaiv ntawm yaj pem hauv ntej. Qhov no ua rau muaj kev cuam tshuam loj lossis stagnation ntawm yaj ntws, ua rau pom tsis zoo nyob rau hauv qhov chaw puv. Txawm li cas los xij, thaum kub kub tseem ntws los ntawm lub rooj vag, cov roj hmab system absorbs thiab khaws lub zog. Thaum lub zog sib sau ua ke mus rau ib theem, nws kov yeej qhov kev tawm tsam ntawm cov yaj hauv pem hauv ntej, ua rau cov yaj kom nthuav dav sai thiab dhia mus rau pem hauv ntej. Tom qab ntawd qhov chaw uas tau sau tshiab yuav muaj qhov ci zoo dua.

Cov roj hmab elastomer ntau dua hauv cov yas, qhov no yuav tshwm sim ntau dua. Cov ntaub ntawv uas tsis zoo toughness tsis tshua muaj pom tsov- kab txaij. Piv txwv li, cov khoom siv txhawb zog, tsis yog -toughened nylon, thiab PBT tsis tshua pom tus tsov- kab txaij thaum lub sij hawm molding, thaum ABS, HIPS, thiab PP cov ntaub ntawv nrog ntxiv EPDM, POE, los yog lwm yam roj hmab Cheebtsam yog heev nquag mus rau tsov - kab txaij defects.

Daim duab 3-54 qhia ib daim duab schematic qhia txog kev tsim cov txheej txheem ntawm tsov kab txaij.

 

info-759-331

 

Kev tshem tawm lossis txo tus Tsov - cov qauv ntawm daim tawv nqaij feem ntau yog hais txog cov txheej txheem molding, xws li nce cov khoom kub, nce pwm kub, thiab txo tus nqi txhaj tshuaj.