Koj puas tau paub tag nrho cov khoom siv yas?

Jan 04, 2023

Tso lus

Cov yas tuaj yeem yog cov ntshiab resin los yog sib tov nrog ntau yam additives. Cov resin ua raws li ib tug binder. Cov additives yog siv los txhim kho lub cev thiab txhua yam khoom ntawm cov ntshiab resin, txhim kho kev ua tau zoo los yog txuag resin.

 

Yog li ntawd, qhov yooj yim tshaj plaws lub cev thiab tshuaj lom neeg cov khoom ntawm plastics yog txiav txim los ntawm cov khoom ntawm resins. Resin tuaj yeem muab faib ua cov khoom siv ntuj tsim thiab cov khoom siv dag zog, tom kawg kuj tseem hu ua hluavtaws cob.

 

Resins yog cov polymers, uas muaj qhov tshwj xeeb sab hauv thiab sab nraud cov qauv molecular. Cov qauv sab hauv ntawm polymer txiav txim siab lub cev thiab cov khoom siv tshuaj lom neeg ntawm polymer; Cov qauv sab nraud ntawm polymer txiav txim siab qhov kev ua tau zoo thiab lub cev thiab cov khoom siv hluav taws xob ntawm polymer.

 

Polymers tuaj yeem muab faib ua cov tsis crystalline (amorphous), semi crystalline thiab crystalline raws li cov qauv thiab morphology ntawm chains tom qab solidification. Yog li ntawd, kuj muaj amorphous thiab crystalline plastics.

 

Thaum lub sij hawm solidification ntawm crystalline plastics, muaj cov txheej txheem los ntawm crystal nucleus mus rau crystal grain, tsim ib lub cev lub xeev. Piv txwv li, PE, PP, PA, POM, thiab lwm yam yog crystalline.

Thaum amorphous plastics solidify, cov txheej txheem kev loj hlob yam tsis muaj siv lead ua nucleus thiab cov nplej tsuas yog "khov" ntawm cov saw dawb macromolecular, xws li PS, PVC, PMMA, PC, thiab lwm yam.

 

 

Raws li kev xav ntawm nws cov plastics ntawm thermal ua, nws tuaj yeem muab faib ua cov thermoplastic thiab thermosetting plastics. Thermoplastic plastics yog tus yam ntxwv los ntawm softening thaum rhuab thiab rov qab mus rau cov khoom thaum txias. Cov txheej txheem thim rov qab no tuaj yeem rov qab tau ntau zaus. Xws li PS, PVC, PA, PP, POM, thiab lwm yam; Lub thermosetting yas yog tus cwj pwm los ntawm kev hloov mus rau hauv cov yas yaj ntawm qhov kub thiab txias. Txawm li cas los xij, yog tias qhov kub thiab txias tseem nce ntxiv, cov polymer sab hauv yuav raug kho vim yog kev sib txuas yog tias lub sijhawm cua sov ntev. Nws tsis tuaj yeem softened mus rau thawj lub xeev los ntawm cua sov, thiab tsis tuaj yeem ua tiav ntau zaus. Xws li epoxy, furan, amino, phenolic, thiab lwm yam.

 

 

Common muab tub lim

 

Common fillers rau kev txhaj tshuaj molding cov ntaub ntawv muaj xws li cov muab tub lim, hlau muab tub lim, organic fillers, luv fiber fillers thiab ntev fiber ntau fillers. Ntxiv cov fillers no tuaj yeem txo tus nqi ntawm cov khoom txhaj tshuaj molding, thiab txhim kho lub cev thiab cov khoom siv dag zog, cov khoom siv tshuaj lom neeg thiab cov khoom siv hluav taws xob los ntawm kev nce nyiaj txiag; Nws tuaj yeem txhim kho cov cuab yeej ua haujlwm, cov cuab yeej rheological, txo cov viscosity thiab txhim kho kev tawg.

Common fillers muaj xws li limestone, calcium carbonate, talc, calcium silicate, mica, aluminium hydroxide, calcium sulfate, thiab cov khoom ua liaj ua teb thiab sab nrauv.

 

Organic fillers yog cov khoom tseem ceeb hauv cov khoom yas tam sim no, suav nrog cov khoom siv ntuj tsim thiab cov khoom siv hluavtaws, suav nrog ntoo, ntoo hmoov, husk ntawm Hu Nu, paj rwb cog cellulose, thiab lwm yam; Cov khoom siv hluavtaws muaj xws li rov siv dua cellulose, xws li: cov ntaub npuag, polyacrylonitrile fiber, nylon fiber, polyester fiber, thiab lwm yam.

Qee cov fillers ntxiv rau cov khoom siv tshuaj molding yuav tsum tau kho nrog kev hloov kho saum npoo. Cov txheej txheem kev kho mob ua raws li qhov kev xav ntawm kev sib txuas chemistry, qhov kev xav ntawm kev ntub dej ntawm cov muab tub lim thiab polymer nto, cov kev xav ntawm acid-base kev sib cuam tshuam, thiab kev sib xyaw txoj kev xav, uas muab cov khoom siv nrog qee yam khoom zoo.

 

Tam sim no, feem ntau siv deg modifiers muaj xws li silane coupling tus neeg saib xyuas, titanate coupling tus neeg saib xyuas, organic silicon kho tus neeg saib xyuas, thiab lwm yam.