1. Khoom taw qhia txog cov yas profile pob khawm.
Peb muaj ntau cov khoom siv sib txawv rau extrude yas, xws li PVC, PE, PP, PC, ABS, PMMA, TPE, thiab lwm yam .Peb ua haujlwm customized ua haujlwm kom tau raws li cov neeg siv khoom siab thiab kev cia siab.
2. Cov khoom lag luam tshwj xeeb cov yas khawm pob khawm.
Cov khoom siv | ABS |
Qhov Coob | 28 hli dav |
xim | ntshiab, semi-meej, opal |
tsim | Tus qauv loj lossis kev cai ua ntau thiab tsawg |
Ntev | Los ntawm 0. 5 meter mus txog 5 meter ntev |
ntim | Kev ntim cov thawv lossis ntoo thawv |
3. Cov yam ntxwv khoom thiab daim ntawv thov ntawm cov yas profile khawm.
Superior cuam tshuam lub zog.
Superior transparency rau kho qhov muag thov.
Huab cua zoo ua hauj.
Lub peev xwm hluav taws xob zoo heev.
Daim ntaub ntawv:
Led Teeb npog / lens.
Hluav taws xob Cheebtsam.
Cov khoom siv kho tsev.
Cov khoom muag: