HIPS Description
1.Scientific lub npe: siab cuam tshuam polystyrene
2.English lub npe: siab feem ntau polystyrene
3.Natural xim: Ntuj xim yog cov khoom siv dawb opaque nrog matt nto, yoog raws, thiab tsis muaj brittleness; nws yog non-toxic thiab tsw.
4.Combustion zog: Nws yog flammable thiab tuaj yeem hlawv tom qab tua hluav taws. Cov nplaim hluav taws sab saud yog golden daj. Thaum kub hnyiab, nws yuav soften thiab ua npuas ncauj, emit tuab pa luam yeeb dub kab nrog ya tshauv, thiab emit tsis muaj kua dripping.
5.Advantages: Vim hais tias polystyrene yog ib qho nyuaj thiab nkig, yooj yim tawg, thiab tsis cuam tshuam resistant, roj hmab hloov txoj kev yog siv los daws cov teeb meem teev saum toj no.
Qhov zoo tshaj plaws ntawm HIPS yog nws lub zog muaj zog, uas yog ntau tshaj plaub npaug ntawm ABS.
Cov rwb thaiv tsev hluav taws xob zoo heev, HIPS yooj yim rau xim thiab luam tawm.
HIPS muaj qhov tawv tawv heev.
6.Disadvantages: Txawm hais tias HIPS muaj lub zog muaj zog, nws qhov elongation tus nqi qis dua li ntawm ABS. Yog li ntawd, tus kheej-tapping screws tuaj yeem yooj yim tawg cov ntsia hlau qhov tsim ntawm lub plhaub. Lub gloss ntawm qhov chaw ua npub vim qhov sib ntxiv ntawm cov khoom siv roj hmab, thiab qhov saum npoo yog npub; HIPS muaj qhov tsis zoo thermal stability thiab tsis tshua muaj cua sov.
Siv rau hauv kev tsim cov vaj tsev rau cov khoom siv hauv tsev.
Rau kev tsim cov khoom siv niaj hnub thiab cov khoom ua si plhaub
Extruded tshuab moulded ntim, hollow cov khoom, thiab lub raj mis
Infusion forming execution Qhov dav dav softening cim ntawm HIPS yog nyob ib ncig ntawm 170 degree, thiab qhov lwj kub yog 260 degree; lub customizable Scope ntawm infusion kub yog nruab nrab loj. Thaum infusion tsim, qhov kev siv dav dav yog 180 degree - - 240 degree ; nyob rau hauv lub teeb ntawm lub xub ntiag ntawm elastic qhov chaw, nws khaws cia ib tug txwv kom muaj nuj nqis ntawm cov dej. Thaum lub sij hawm tsim, nws yuav tsum tau yaum kom qhuav, thiab tuaj yeem qhuav ntawm 80-90 degree rau 1-2 teev; HIPS yog vim qhov elastic.
Yog li ntawd, qhov sib xyaw ua ke ntawm HIPS yuav tsum tsis txhob raug tso tseg rau hauv lub siab ntawm lub siab thaum lub sij hawm infusion, thiab lub liquefy thickness yog siab tshaj li ntawm PS, txawm li cas los xij cov kev nkag thiab sprinter yog dav dav thiab tuaj yeem thauj khoom nrog cov khoom; cov khoom yog inclined rau hluav taws xob tsim los ntawm kev sib txhuam, thiab qhov chaw tsis yooj yim rau assimilate hmoov av. Shrinkage tus nqi yog 5‰; dej nyab esteem yog 0.05mm
Khoom duab piv txwv: